C15E4合金钢圆钢可以按照规格切割【萌日金属】
特 殊 钢:哈氏合金,镍基合金,蒙乃尔合金,高温合金,HastelloyC-276,HastelloyC-22,Monel 400,Monel K500,Inconel600,Inconel625,Incoloy800,Incoloy825,GH2132。
合金结构钢:300M钢、40CrNi2Si2MoV、SNCM439、40CrNiMoA,20CrNi2Mo ,20CrMnMo ,40CrMnMo ,35CrMo ,42CrMo,4140,4130,SAE8620,45CrNiMoVA,16MnCr5(15CrMn),38CrMoAlA,20MnCr5(20CrMn),18Cr2Ni4WA ,12CrNi3,20Cr2Ni4A ,35CrMnSiA,30CrMnSiA,18CrNi3Mo,25Cr2MoV,22CrMoH,20CrMnMo,20-30CrMnTi,25CrNiMoV,20CrNiMo,G20CrNi2MoCr12,Cr12MoV,Cr12Mo1V1,H13,718#,P20,5CrNiMo,5CrMnMo,CrWMn,9CrSi,9Cr2,5-6CrW2Si,8Cr3,9Mn2V,4Cr5W2VSi,30Cr3W,4Cr2MoVNi(B2),SKD11.,30Cr2Ni2Mo,17Cr2Ni2Mo,17CrNiMo6,18CrNiMo7,34CrNiMo6,30CrNiMo8,40-45CrNi,20Ni4Mo,20-30CrMnSiNi2A,38CrSi,34CrNi1Mo,12CrNi3A,20CrNi 30CrNi3A,34-37CrNi3A,34-37CrNi3MoA,12Cr2Ni4A,20Cr2Ni4A,18-25Cr2Ni4W,25Cr2MoV,25Cr2Mo1V,12CrMo,12Cr1MoV,35CrMoV,45Cr2MoV,18CrNi3MoA,20CrNi3MoA,25CrNi3MoA,,22SiMnCrNi2MoVA,5CrW2Si.等。
14、铜(Cu):武钢用大冶矿石所炼的钢,往往含有铜。铜能提高强度和韧性,特别是大气腐蚀性能。缺点是在热加工时容易产生热脆,铜含量超过0.5%塑性显著降低。当铜含量小于0.50%对焊接性无影响。
碳钢也叫碳素钢,含碳量WC小于2%的铁碳合金。碳钢除含碳外一般还含有少量的硅、锰、硫、磷 按用途可以把碳钢分为碳素结构钢、碳素工具钢和易切削结构钢三类。碳素结构钢又分为建筑结构钢和机器制造结构钢两种 按含碳量可以把碳钢分为低碳钢(WC ≤ 0.25%),中碳钢(WC0.25%——0.6%)和高碳钢(WC>0。6%) 按磷、硫含量可以把碳素钢分为普通碳素钢(含磷、硫较高)、优质碳素钢(含磷、硫较低)和高级优质钢(含磷、硫更低) 一般碳钢中含碳量较高则硬度越高,强度也越高,但塑性较低。
耐热钢 1、低碳高合金钢;2、耐热性能好;3、用于耐热材料、部分可做抗腐蚀材料。
一、 齿轮、轴用钢:20CrMnMo、20CrNiMo、8620、G20CrNiMo、20CrNi2Mo、24Cr13V、17Cr2Ni2Mo、17CrNiMo6、18CrNiMo7、4Cr13、30CrNiMo8、GCr4、GCr15、GCr15SiMn、GCr15SiMo、GCr18Mo、G20CrMoG20CrNiMo、G20Cr2Ni4、G10CrNi3Mo、G20Cr2Mn2Mo 、25Cr2MoV 、25Cr2Mo1V 、12Cr1MoV
模具钢:Cr12,Cr12MoV,Cr12Mo1V1,H13,718#,P20,5CrNiMo,5CrMnMo,CrWMn,9CrSi,9Cr2,5-6CrW2Si,8Cr3,9Mn2V,4Cr5W2VSi,30Cr3W,4Cr2MoVNi(B2),SKD11.
C15E4合金钢圆钢可以按照规格切割【萌日金属】